News

How can cracking be prevented when forming large cylindrical battery cans?

Cracking during the forming of large cylindrical battery cans is primarily prevented through a combination of correct material selection, precise process parameter control, and appropriate press technology. The deeper and wider the can, the greater the strain placed on the metal, making each of these factors more critical at larger formats such as 46xx cells. The sections below address the specific questions that matter most when planning or optimizing a battery can forming line.

What causes cracking in large cylindrical battery cans during forming?

Cracking in large cylindrical battery cans occurs when tensile stress in the metal exceeds the material’s formability limit during deep drawing. This typically happens at the can wall or at the transition between the base and the wall, where the material is stretched most severely. Larger formats such as the 4680 cell amplify this risk because the drawing ratio increases significantly compared with smaller formats like 18650 or 21700.

The root causes of battery can cracking fall into several interconnected categories. Excessive drawing ratio is the most common structural cause: when the diameter of the blank relative to the diameter of the finished can is too high for a single forming stage, the material cannot flow freely enough and fractures under tension. Insufficient blank holder force allows the material to wrinkle rather than flow smoothly, which in turn causes localized thinning and eventual cracking. Conversely, too much blank holder force restricts material flow entirely, producing the same fracture outcome through a different mechanism.

Forming speed also plays a direct role. At excessively high cycle rates without adequate lubrication or tool geometry, frictional heat builds up at the die radius, reducing the material’s local ductility and triggering surface cracks. For large-format cans, where the forming path is longer and the wall area exposed to friction is greater, this effect is more pronounced than in smaller cell formats.

How does material selection affect cracking risk in battery can production?

Material selection is one of the most direct levers for controlling cracking risk in battery can forming. Nickel-plated steel is the standard material for cylindrical battery cans because it combines adequate tensile strength with the ductility required for multi-stage deep drawing, while also providing the electrochemical compatibility and corrosion resistance that battery cell chemistry demands.

Within nickel-plated steel grades, the key properties that determine cracking susceptibility are the r-value (normal anisotropy), the n-value (strain hardening exponent), and the material’s overall elongation at break. A high r-value means the material resists thinning in the thickness direction and instead flows laterally, which is exactly the behavior needed in deep drawing. A high n-value means the material distributes strain more evenly across the wall rather than concentrating it at the weakest point.

For large-format cans, these material properties become more demanding because the forming depth is greater and the number of redraw stages required is higher. Each redraw stage work-hardens the material progressively, reducing the remaining ductility available for subsequent stages. Selecting a steel grade with sufficient initial ductility to survive the full forming sequence without intermediate annealing is therefore a critical planning decision. Material consistency across coils also matters: variations in thickness, surface quality, or mechanical properties between batches can cause cracking to appear intermittently, making the root cause harder to diagnose.

What process parameters control crack formation in deep drawing?

The process parameters that most directly control crack formation in deep drawing of battery cans are blank holder force, drawing ratio per stage, lubrication, punch and die radius, and drawing speed. Optimizing these parameters in combination, rather than individually, is what separates a stable high-volume process from one that produces intermittent scrap.

Blank holder force and drawing ratio

Blank holder force must be calibrated precisely for each material grade and can geometry. Too little force allows wrinkling in the flange area, which then causes the wrinkled material to be pulled into the die gap and crack. Too much force locks the material and prevents the controlled inward flow that distributes strain across the wall. For large-format cans, the blank holder force window is narrower because the flange area is larger and the material must travel further before the draw is complete.

The drawing ratio per stage should be kept within the material’s proven limit. Rather than attempting to achieve the full can depth in one or two stages, a well-designed process distributes the total reduction across multiple redraw stages. Each stage removes a portion of the total strain, keeping the cumulative stress within the material’s ductility envelope at every point in the sequence.

Lubrication and tool geometry

Effective lubrication reduces friction between the punch, die, and material surface, lowering the tensile load required to draw the cup and reducing the risk of surface cracking caused by frictional heat. The die radius and punch radius must be matched to the material thickness and the drawing ratio: too tight a radius concentrates bending stress, while too generous a radius can allow wrinkling. For large-format cans, maintaining consistent lubrication across a wider blank surface requires careful attention to lubricant application systems integrated into the line.

How does press technology influence cracking outcomes for large-format cans?

Press technology influences cracking outcomes by determining how precisely and consistently the forming force, speed, and position are controlled throughout each stroke. For large cylindrical battery cans, where the forming sequence is longer and the tolerance for process variation is tighter, the choice of press type has a measurable impact on scrap rates and wall quality.

Conventional mechanical presses deliver their maximum force only near bottom dead center. This means that during the earlier part of the stroke, where the blank is being drawn into the die and the risk of cracking is already present, the available force control is limited. Servo-driven press systems address this directly by allowing force and speed to be programmed independently at any point in the stroke. This makes it possible to slow the forming speed through the most critical phase of the draw, reduce the peak tensile load on the material, and hold the punch at a defined position for a dwell period if the process requires it. Our Servo Spindle Press technology delivers maximum press force at any stroke position, not only at bottom dead center, which opens up forming strategies that are simply not available on conventional mechanical equipment.

For high-volume production, the repeatability of press motion is equally important. A press that introduces even small variations in stroke position or speed from cycle to cycle will produce corresponding variation in wall thickness and forming stress, which eventually manifests as intermittent cracking. Active ram position control, which compensates in real time for frame deflection under load, keeps the forming geometry consistent across every stroke and across long production runs.

What tooling design factors help prevent cracking in battery can forming?

Tooling design is the physical interface between the press and the material, and it directly determines where stress concentrates during forming. For large cylindrical battery cans, the most important tooling factors are die radius, punch radius, die clearance, blank holder geometry, and surface finish of all contact surfaces.

The die entry radius controls how smoothly the material bends and unbends as it flows over the die shoulder. A radius that is too small creates a sharp bending load that thins the material locally and initiates cracks. A radius that is too large reduces the die’s ability to control material flow, leading to wrinkling. The correct radius is a function of material thickness and the drawing ratio for that stage, and it must be recalculated for each redraw stage rather than carried over from the first draw.

Die clearance, the gap between the punch and the die wall, must be matched to the material thickness at each stage. As the material is redrawn, it thins slightly, and the clearance must account for this reduction. Insufficient clearance causes ironing, which thins the wall further and can trigger cracking. Excessive clearance allows the material to wrinkle within the die gap.

Surface finish on the punch, die, and blank holder affects friction and therefore the tensile load the material must sustain during forming. Polished surfaces with consistent finish reduce friction and extend tool life. For large-format cans, where the total contact area between tool and material is greater, surface quality has a proportionally larger effect on forming stability and crack risk.

When should manufacturers consider a cupping press for large battery can production?

Manufacturers should consider a dedicated cupping press when producing large cylindrical battery cans in high volumes where the first forming stage, converting a flat metal blank into a precise cup, must be performed at speed, with tight dimensional consistency, and in a way that sets up every subsequent redraw stage for success. The cup geometry produced in the first stage directly determines the forming conditions in all following stages, making the quality of the cupping operation foundational to the entire process.

A cupping press combines blanking and cupping in a single machine stroke. Multiple blanks are punched from a wide metal strip simultaneously, and then each blank is immediately formed into a cup within the same stroke cycle. This approach maximizes material utilization, eliminates the handling step between blanking and cupping, and produces a cup with consistent geometry that is dimensionally compatible with downstream redraw equipment. For large battery can formats, where the blank diameter is significantly larger and the cup depth is greater, this integrated approach reduces the number of process handovers and the associated risk of dimensional variation entering the redraw sequence.

Our cupping and redraw press systems are designed specifically for this production logic. Each system is individually configured to the strip width, sheet thickness, cup geometry, and target output rate required by the customer’s specific battery can format.

How H&T Helps Prevent Cracking in Large Cylindrical Battery Can Production

We supply complete battery can production lines engineered to address the cracking risks described throughout this article, from the first blanking stroke through to the finished can geometry. Our approach combines cupping equipment, multiple redraw stages, and integrated automation into a coordinated system that maintains process stability across high-volume production runs for formats including 18650, 21700, and 46xx cells.

Here is what our production line technology delivers specifically for cracking prevention:

  • Controlled blank holder force at the cupping stage, configured precisely for the material grade and cup geometry, ensuring consistent material flow from the first stroke
  • Multi-stage redraw sequences that distribute the total forming reduction across multiple steps, keeping strain within the material’s ductility limit at every stage
  • Servo press capability that allows forming speed and force to be programmed independently at any point in the stroke, enabling gentler processing through the most critical phases of the draw
  • Active ram position control that compensates in real time for frame deflection, maintaining consistent die clearance and forming geometry across every cycle
  • Integrated camera and quality inspection systems that detect dimensional deviations and surface defects in-line, before defective parts progress further through the process
  • Buffer systems between production stages that prevent a single machine event from stopping the entire line, maintaining throughput and process stability
  • Tool and process chain design support, including die radius selection, clearance configuration, and lubrication system integration, tailored to the specific battery can format and material specification

Our servo spindle press systems are particularly well suited to large-format battery can production where conventional mechanical presses reach the limits of their force and position control. Whether you are planning a new production line or evaluating upgrades to an existing process, we offer individual consulting, complete system design, and comprehensive after-sales support. Contact us to discuss your battery can format requirements and find out how we can help you achieve stable, high-volume production with minimal scrap.

Related Articles